Vacuum Sintering-A Way to Improve Ductility and Toughness of Structural P/M Parts at the Right Price
Most parts fabricators do not understand the importance of a quality sinter to provide improved ductility and toughness for tomorrow’s markets. As a result, the potential for growth markets for quality parts has seldom been exploited. Today the main emphasis is still on cost reduction, rather than quality.
Authors: Kenneth H. Moyer, Magna-Tech P/M Labs, Ronald D. Payne, Sinteris PM Corporation