Vacuum Heat Treating Services
Heat Treating Metals with Quality You Can Rely On
Vacuum Heat Treating and Brazing Services
What is Vacuum Heat Treating?
Solar Atmospheres’ vacuum heat treating is a highly controlled thermal processing method in which metal components are heated inside a sealed vacuum furnace. By removing air from the chamber, oxidation is eliminated, producing clean, bright surfaces while enhancing critical material properties such as strength, hardness, and durability, preserves the integrity of your components. These benefits make vacuum heat treating ideal for demanding applications in aerospace, defense, medical, and precision tooling industries.
The process allows precise control of heating and cooling rates and often incorporates inert gas quenching—such as argon or nitrogen—to achieve consistent results with minimal distortion. Compared to conventional heat treating methods, vacuum processing delivers superior metallurgical quality, tighter tolerances, and improved part performance.
Don’t let contaminants compromise your results—partner with a leader in advanced vacuum heat treatment solutions.
The Importance of Heat Treating Metals with Quality You Can Rely On
Add value to your parts by leveraging Solar Atmospheres’ vacuum heat treating services with our unmatched technical expertise, quality and world-class equipment. Solar uses advanced vacuum heat treating techniques to improve performance, strength and toughness. With our extensive range of processes, and over 100 furnaces for vacuum heat treating and brazing services, ranging from lab-size research and development furnaces to the largest commercial vacuum furnace (48 feet long, 150,000 pound capacity), you will realize innovative and efficient solutions. From bearings to blades and beyond, partner with Solar Atmospheres for results that exceed your expectations. Get reliable turnaround with responsive customer service, and coast-to-coast, 24/7 operations.
What are the Reasons for Heat Treating Metal?
- Remove stresses, such as those developed in processing or manufacturing
- Refine the grain structure of the metal
- Improves the economical grade of metal to use in place of something more expensive
- Increase tensile, toughness, strength and ductility
- Improves machineability and weldability
- Improves wear performance
- Improves the cutting properties of tool steels
- Improves corrosion resistance in stainless materials
- Change or modify magnetic properties
Unlock the Benefits of Advanced Heat Treatment with Our Cutting-Edge Vacuum Furnace Technology
Many heat treatment processes benefit from our innovative vacuum furnace technology, engineered by our sister company, Solar Manufacturing. These state-of-the-art furnaces are specifically designed to create the optimal atmosphere for heating and cooling metals, ensuring precision and quality in every treatment.
Our vacuum furnace technology supports a wide range of processes, including:
- Annealing
- Age Hardening
- Stress Relieving
- Hardening and Tempering
- Degassing
- Vacuum Oil Quenching
- Vacuum Brazing
- Low Pressure Carburizing
- Nitriding
- Creep Forming
- Hydriding/Dehydriding
Experience the next level of heat treating with our cutting-edge vacuum furnace technology.
Maximize Safety with Vacuum Heat Treatment
Safety is paramount when it comes to metal treatment, and vacuum heat treatment is one of the safest methods available. Unlike other processes, vacuum heat treatment eliminates the need for flammable gases, is completely free of pollution and oxygen exposure, and prevents contamination from harmful particles.
This treatment method is not only highly efficient but also free from health hazards, helping you maintain a safe work environment. By choosing vacuum heat treatment, you can more easily stay OSHA compliant and protect the well-being of your employees, all while ensuring high-quality results.
Components Processed
- Aircraft parts and equipment
- Power Generation blades and components
- Medical devices
- Implants
- Tooling
- Gears
- Braze assemblies
- Plate
- Forgings
- Bar
- Ingots
- Weldments
- Structural Components
- Castings
- Sheet
- Tube and pipe
. . . and more
Materials Processed
- Alloy Steels
- Titanium
- Stainless Steel
- Precipitation Hardening Stainless Steel (PH)
- Inconel
- Nickel Based Alloys
- Tantalum
- Niobium
- Nitinol
- Hiperco 50/50A
- AerMet® 100
- Tungsten
- Zirconium
- Tool Steel
- High Speed Tool Steels
- Hot Working Tool Steels
- Copper
- Brass
. . . and more
Vacuum Heat Treating Services
Select a heat treating service below to find out more. For clarification of terms, please visit our heat treating glossary.
NEWS
-
Solar Atmospheres of San Diego Earns 24-Month Nadcap Merit Status for Vacuum Heat Treating and Brazing
-
Solar Atmospheres of California Announces Promotion of Courtney Castillejos to Quality Manager
-
Solar Atmospheres of Western PA Expands Titanium Processing Capabilities with New Water Quench Furnace