Partial Pressure Vacuum Processing – Part II: Applications
This article is based on a presentation at the Furnaces North America ’96 Conference, held in Dearborn, MI, September 24-26, 1996 and sponsored by Industrial Heating. In part two, partial pressure vacuum processing cycles for different materials are reviewed. Information regarding the evaporation of base metals and reactive processing was presented in the September ’97 issue of Industrial Heating.
Author:
Originally Published: Industrial Heating, September 1997
Download: Partial Pressure Vacuum Processing – Part II: Applications