Utilization of Vacuum Heat Treating Technology for Refractory Metal, Titanium and their Alloys for Powder Applications

Increased usage of refractory metals, titanium and their alloys in the aerospace and electronics industries has led to the use of the hydride/dehydride (HDH) heat treating process for recovery of spent materials.  The HDH process has been known for many years in the manufacturing of transition-metal powders.

 

Author: 

Dr. Virginia Osterman, Corporate Chemist

Originally Published: Industrial Heating, May 2008

 


Download Utilization of Vacuum Heat Treating Technology for Refractory Metal, Titanium and their Alloys for Powder Applications Paper