Calculating the Gas Flow Rate for Vacuum Carburization
A proposed technique of determining the actual required flow rate of the carburizing gas into a furnace to provide the necessary amount of carbon for a given work load.
Author: Harry W. Antes, Consultant-Solar Atmospheres
Originally Published: Heat Treating Progress, August 2005
Download Calculating the Gas Flow Rate for Vacuum Carburization Paper