Furnace Capabilities

Furnace Capabilities

Our unique relationship with Solar Manufacturing gives Solar Atmospheres unparalleled access to state-of-the-art vacuum furnace technology and industry-leading innovation. As Solar Atmospheres monitors the operation of over 90 different vacuum furnaces that run 24/7, year-round, ideas for improving performance and durability get fed back to the engineers at our sister company. Many new designs for graphite insulation, curved graphite heating elements, tapered gas nozzles, high velocity gas quench systems, and energy management were born from this cooperative connection. Knowing vacuum heat treating inside and out, paired with decades of processing expertise of our founder, engineers, and metallurgists, allows Solar Manufacturing to produce the most technically advanced and highest performing furnaces on the market.

 

*Note: Part sizes and weight can exceed the dimensions and capability given based on placement and configuration in the furnace. Please contact a Solar sales engineer to determine if your parts can be processed.

Vacuum Furnace Sizes

  Furnace #    Hot Zone Dimensions   Max Temperature   Max Load (lbs)
 HT-20  14″ wide X 12″ high  2400°F / 1315°C  50
 HT-66  8″ dia. X 12″ deep  3000°F / 1649°C  100
 HT-129  12″ wide x 12″ high x 18″ deep  2400°F / 1315°C  250
 HT-148  12″ wide x 12″ high x 18″ deep (all metal hot zone)  2400°F / 1315°C  250
 HT-106  12″ wide X 11″ high X 20″ deep  2400°F / 1315ºC  200
 HT-48  14″ wide X 12″ high X 30″ deep  2650°F / 1454°C  750
 HT-61  14″ wide X 12″ high X 30″ deep (10 bar)  2650°F / 1454°C  750
 HT-46  12″ wide X 12″ high X 35″ deep  3450°F / 1900°C  200
 HT-158  18″ wide X 18″ high X 36″ deep (all metal hot zone)  2400°F / 1315°C  1,000
 HT-10  24″ wide X 24″ high X 36″ deep  2800°F / 1538°C  1,500
 HT-23  24″ wide X 24″ high X 36″ deep  2800°F / 1538°C  1,500
 HT-1  24″ wide X 24″ high X 36″ deep (all metal hot zone)  2400°F / 1315°C  1,500
 HT-125  24″ wide X 24″ high X 36″ deep (all metal hot zone)  2400°F / 1315°C  1,500
 HT-31  24″ wide X 24″ high X 36″ deep (10 bar)  2650°F / 1454°C  1,500
 HT-162 24″ wide X 24″ high X 72″ deep (20 bar)  2400°F / 1315°C  2,000
 HT-36  36″ wide X 30″ high X 48″ deep  3000°F / 1649°C  3,500
 HT-105  36″ wide X 36″ high X 48″ deep (all metal hot zone)  2400°F / 1315°C  3,500
 HT-136  36″ wide X 36″ high X 48″ deep (all metal hot zone)  2400°F / 1315°C  3,500
 HT-5  40″ wide X 30″ high X 50″ deep  2800°F / 1538°C  4,000
 HT-107  40″ wide X 30″ high X 50″ deep  2800°F / 1538°C  4,000
 HT-77  36″ wide X 36″ high X 50″ deep  2650°F / 1454°C  3,500
 HT-86  36″ wide X 36″ high X 50″ deep  2650°F / 1454°C  3,500
 HT-28  36″ wide X 36″ high X 50″ deep (6 bar)  2650°F / 1454°C  3,500
 HT-27  40″ wide X 36″ high X 50″ deep  2650°F / 1454°C  3,500
 HT-44  40″ wide X 36″ high X 50″ deep (10 bar)  2650°F / 1454°C  3,500
 HT-72  24” wide X 24” high X 72” deep (10 bar)  2400°F / 1315ºC  1,500
 HT-103  24” wide X 24” high X 72” deep (10 bar)  2400°F / 1315ºC  1,500
 HT-14  48″ wide X 40″ high X 72″ deep  2800°F / 1538°C  6,000
 HT-150  48″ wide X 40″ high X 72″ deep  2800°F / 1538°C  6,000
 HT-178  48″ wide X 40″ high X 72″ deep  2800°F / 1538°C  6,000
 HT-179  48″ wide X 40″ high X 72″ deep  2800°F / 1538°C  6,000
 HT-58  48″ wide X 40″ high X 72″ deep (10 bar)  2650°F / 1454°C  10,000
 HT-131  48″ wide X 40″ high X 72″ deep (10 bar)  2650°F / 1454°C  10,000
 HT-13  60″ wide X 48″ high X 120″ deep  2650°F / 1454°C  10,000
 HT-33  54″ wide X 54″ high X 144″ deep  2650°F / 1454°C  15,000
 HT-183  54″ wide X 54″ high X 144″ deep  2650°F / 1454°C  15,000
 HT-73  54″ wide X 54″ high X 144” deep  2400°F / 1315°C  50,000

Gas Nitriding Furnace Sizes

 Furnace #   Hot Zone Dimensions  Max Temperature  Max Load (lbs)
 HT-65  7″ dia. X 12″ high
 3000°F / 1650°C
 100
 HT-81  33″ wide X 32″ high X 47″ deep
 1400°F / 760°C
 2,500
 HT-138  33″ wide X 32″ high X 47″ deep
 1400°F / 760°C
 2,500

Air Tempering Furnace Sizes

 Furnace #   Hot Zone Dimensions  Max Temperature  Max Load (lbs)
 HT-12  18″ wide X 15″ high X 19″ deep  550°F / 287°C  50
 HT-24  19″ wide X 18″ high X 19″ deep  1200°F / 649°C  750
 HT-25  19″ wide X 18″ high X 19″ deep  1200°F / 649°C  750
 HT-71  24″ wide X 24″ high X 36″ deep  1200°F / 649ºC  500
 HT-21  24″ wide X 24″ high X 48″ deep  1350°F / 732°C  1,500
 HT-34  48″ wide X 39″ high X 54″ deep  1400°F / 760°C  5,000
 HT-101  53″ wide X 40″ high X 60″ deep  1350°F / 732°C  5,000
 HT-140  60″ wide X 48″ high X 168″ deep   1400°F / 760°C  30,000

Cryogenic Freezer Sizes

 Freezer#   Hot Zone Dimensions  Max Temperature  Max Load (lbs)
 DF-16
 18″ wide X 18″ high X 18″ deep
 -120°F / -85°C
 1,000
 DF-15
 24″ wide X 24″ high X 48″ deep
 -300°F / -184°C
 2,000
 DF-91
 52″ wide X 23″ high X 27″ deep
 -300°F / -184°C
 250
 DF-94
 52″ wide X 52″ high X 96″ deep
 -300°F / +500°F
 10,000
 DF-130
 34″ wide X 39″ high X 70″ deep
 -120°F / -85°C
 1,000

Vacuum Furnace Sizes

 Furnace #   Hot Zone Dimensions  Max Temperature  Max Load (lbs)
 HT-102  12″ wide X 12″ high X 18” deep  2500°F / 1370°C  250
 HT-62  18″ wide X 14″ high X 28″ deep (10 bar)  2650°F / 1454°C  750
 HT-50  24″ wide X 24″ high X 36″ deep (10 bar)  2650°F / 1454°C  1,500
 HT-128  24″ wide X 24″ high X 36″ deep (all-metal hot zone)  2500°F / 1370°C  1,500
 HT-186  24″ wide X 24″ high X 36″ deep (all metal hot zone)  2500°F / 1370°C  1,500
 HT-51  40″ wide X 36″ high X 50″ deep (10 bar)  2650°F / 1454°C  3,500
 HT-97  40″ wide X 36″ high X 50″ deep (20 bar)  2650°F / 1454°C  5,000
 HT-69  68″ wide X 84″ high X 74″ deep  2100°F / 1149°C  15,000
 HT-70  48″ wide X 39″ high X 96″ deep  2650°F / 1454°C  6,000
 HT-146  48″ wide X 39″ high X 96″ deep (10 bar)  2650°F / 1454°C  6,000
 HT-68  54″ wide X 54″ high X 144″ deep  2800°F / 1538°C  50,000
 HT-49  54″ wide X 54″ high X 288” deep  2650°F / 1454°C  50,000
 HT-74  54″ wide X 54″ high X 288” deep  2650°F / 1454°C  50,000
 HT-78  54″ wide X 54″ high X 288” deep  2650°F / 1454°C  50,000
 HT-79  54″ wide X 54″ high X 432” deep  2650°F / 1454°C  150,000
 HT-119  54″ wide X 54″ high X 576″ deep  2400°F / 1315ºC  150,000

Vacuum Oil Quench Furnace Sizes

  Furnace #   Hot Zone Dimensions   Max Temperature   Max Load (lbs)
 HT-151  40″ wide X 36″ high X 48″ deep  2100°F / 1149ºC  2,000

Air Tempering Furnace Sizes

  Furnace #    Hot Zone Dimensions   Max Temperature   Max Load (lbs)
  HT-54  24″ wide X 24″ high X 36″ deep  1200°F / 649ºC  1,500
  HT-152  36″ wide X 36″ high X 48″ deep  1300°F / 704ºC  3,000
  HT-153  36″ wide X 36″ high X 48″ deep  1300°F / 704ºC  3,000
  HT-53  48″ wide X 39″ high X 60″ deep  1400°F / 760°C  5,000
  HT-115  48″ wide X 60″ high X 60″ deep  1300°F / 704ºC  10,000
  HT-220  48″ wide X 60″ high X 60″ deep  1400°F / 760°C  5,000
  HT-137  60″ wide X 60″ high X 168″ deep  1450°F / 788ºC  30,000
  HT-180  60″ wide X 60″ high X 168″ deep  1450°F / 788ºC  30,000
  HT-134  60″ wide X 60″ high X 240″ deep  1450°F / 788ºC  30,000

Freezer & Air Temper Furnace Size

  Furnace #    Hot Zone Dimensions   Min / Max Temperature   Max Load (lbs)
 HT-123
 43″ wide X 39″ high X 54″ deep
 -300°F / 1200°F  3,000

Cryogenic Freezer Sizes

  Freezer#    Hot Zone Dimensions   Max Temperature   Max Load (lbs)
 DF-75
  40″ wide X 40″ high X 52″ deep
  -300°F / -184°C   5,000
 DF-156
  48″ wide X 48″ high X 96″ deep
  -300°F / -184°C   10,000

Vacuum Furnace Sizes

  Furnace #    Hot Zone Dimensions   Max Temperature   Max Load (lbs)
 HT-95  8″ wide X 8″ high X 12″ deep  2400°F / 1315ºC  50
 HT-157  12″ wide X 12″ high X 20″ deep  2400°F / 1315ºC  250
 HT-161  12″ wide X 12″ high X 20″ deep  2400°F / 1315ºC  250
 HT-100  12″ wide X 11″ high X 20″ deep (all metal hot zone)  2400°F / 1315ºC  200
 HT-87  36″ wide X 24″ high X 48” deep  2650°F / 1454°C  5,000
 HT-126  36″ wide X 36″ high X 48” deep (10 bar)  2650°F / 1454°C  5,000
 HT-96  36″ wide X 36″ high X 50″ deep (10 bar)  2650°F / 1454°C  5,000
 HT-83  24” wide X 24” high X 72” deep (10 bar)  2400°F /1315ºC  3,500
 HT-127  48″ wide X 48″ high X 72” deep (10 bar)  2650°F / 1454°C  10,000
 HT-132  48″ wide X 48″ high X 72” deep (all metal hot zone)  2650°F / 1454°C  10,000
 HT-182  48″ wide X 48″ high X 96” deep (10 bar)  2650°F / 1454°C  12,000
 HT-108  54″ wide X 54″ high X 144″ deep  2650°F / 1454°C  20,000
 HT-139  54″ wide X 54″ high X 144″ deep  2650°F / 1454°C  50,000
 HT-84  54″ wide X 54″ high X 288” deep  2650°F / 1454°C  50,000

Air Tempering Furnace Sizes

  Furnace #    Hot Zone Dimensions   Max Temperature   Max Load (lbs)
 HT-111  21″ wide X 23″ high X 14″ deep  500°F / 260ºC  150
 HT-99  21″ wide X 21″ high X 23″ deep  1200°F / 649ºC  500
 HT-117  36″ wide X 40″ high X 48″ deep  1700°F / 927ºC  4,000
 HT-89  48″ wide X 48″ high X 72″ deep  1200°F / 649ºC  3,500
 HT-143  48″ wide X 48″ high X 72″ deep  1600°F / 871ºC  10,000
 HT-144  48″ wide X 48″ high X 72″ deep  1600°F / 871ºC  10,000
 HT-160  68″ wide X 48″ high X 168″ deep  1450°F / 788ºC  30,000

Cryogenic Freezer Sizes

  Freezer#    Hot Zone Dimensions   Max Temperature   Max Load (lbs)
 DF-88
 48″ wide X 48″ high X 72″ deep
 -300°F / -184°C
 2,500

Vacuum Furnace Sizes

 Furnace #   Hot Zone Dimensions  Max Temperature  Max Load (lbs)
 HT-113  24″ wide X 24″ high X 36″ deep (10 bar)  2500°F / 1370°C  1,500
 HT-112  36″ wide X 36″ high X 48″ deep  2500°F / 1370°C  5,000
 HT-109  36″ wide X 36″ high X 48″ deep (10 bar)  2500°F / 1370°C  5,000
 HT-184  48″ wide X 48″ high X 96″ deep (10 bar)  2500°F / 1370°C  12,000
 HT-110  54″ wide X 54″ high X 288″ deep  2500°F / 1370°C  50,000
 HT-141  54″ wide X 54″ high X 144″ deep  2500°F / 1370°C  50,000

Air Tempering Furnace Sizes

  Furnace #    Hot Zone Dimensions   Max Temperature   Max Load (lbs)
 HT-147  30″ wide X 29″ high X 25″ deep  1110°F / 593ºC  100
 HT-118  36″ wide X 36″ high X 48″ deep  1250°F / 677ºC  5,000
 HT-98  40″ wide X 36″ high X 144″ deep  1200°F / 649ºC  10,000
 HT-114  60″ wide X 60″ high X 60″ deep  1250°F / 677ºC  7,000

Cryogenic Freezer Sizes

  Freezer#   Hot Zone Dimensions   Max Temperature
 DF-120
 48″ wide X 48″ high X 96″ deep
 -300°F / -184°C

Vacuum Furnace Sizes

  Furnace #    Hot Zone Dimensions   Max Temperature   Max Load (lbs)
 HT-177  12″ wide X 12″ high X 18” deep (all metal hot zone)  2500°F / 1370°C  250
 HT-163  12″ wide X 18″ high X 26″ deep  2650°F / 1454ºC  500
 HT-164  24″ wide X 18″ high X 38″ deep  2500°F / 1370ºC  2,500
 HT-165  24″ wide X 23″ high X 38” deep  2100°F / 1149°C  3,000
 HT-174  36″ wide X 36″ high X 48″ deep  2500°F / 1370°C  5,000
 HT-166  38″ wide X 28″ high X 50” deep  2650°F / 1454°C  5,000
 HT-167  38″ wide X 28″ high X 72″ deep  2650°F / 1454°C  5,000
 HT-168  48” wide X 34” high X 73” deep  2800°F /1538ºC  5,000
 HT-169  48″ wide X 34″ high X 73” deep  2650°F / 1454°C  5,000
 HT-170  54″ wide X 54″ high X 120” deep
 2650°F / 1454°C  10,000

Air Tempering Furnace Sizes

  Furnace #    Hot Zone Dimensions   Max Temperature   Max Load (lbs)
 HT-153  36″ wide X 36″ high X 48″ deep  1300°F / 704ºC  3,000
 HT-171  26″ wide X 40″ high X 26″ deep  1400°F / 760ºC
 HT-172  54″ wide X 46″ high X 54″ deep  1450°F / 788ºC
 HT-215  66″ wide X 48″ high X 168″ deep  1400°F / 760ºC 30,000

Cryogenic Freezer Sizes

  Freezer#    Hot Zone Dimensions   Max Temperature   Max Load (lbs)
 DF-173
 20″ wide X 28″ high X 36″ deep
 -120°F / -85°C
 1,000
 DF-217
 42″ wide X 36″ high X 60″ deep
 -300°F / -184°C

Vacuum Furnace Sizes

  Furnace #    Hot Zone Dimensions   Max Temperature   Max Load (lbs)
 HT-187  15″ wide X 10″ high X 24″ deep  2450°F / 1343°C
 HT-188  48″ wide X 48″ high X 63” deep  2450°F / 1343°C
 HT-189  54″ wide X 54″ high X 58″ deep  2450°F / 1343°C
 HT-190  36″ wide X 36″ high X 48″ deep  2450°F / 1343°C
 HT-191  36″ wide X 36″ high X 48” deep  2450°F / 1343°C
 HT-192  48″ wide X 48″ high X 60” deep  2400°F / 1315°C
 HT-193  48″ wide X 48″ high X 60” deep  2400°F / 1315°C

Air Tempering Furnace Sizes

  Furnace #    Hot Zone Dimensions   Max Temperature   Max Load (lbs)
 HT-197  15.5″ dia. X 16″ deep  1200°F / 649ºC
 HT-198  24″ wide X 16″ high X 18″ deep  850°F / 454ºC
 HT-199  48″ wide X 72″ high X 48″ deep  750°F / 399ºC
 HT-200  24″ wide X 16″ high X 18″ deep  850°F / 454ºC
 HT-201  27″ dia. X 30″ deep  1200°F / 649ºC
 HT-202  24″ wide X 20″ high X 48″ deep  1400°F / 760ºC
 HT-203  24″ wide X 18″ high X 42″ deep  2250°F / 1232ºC
 HT-204  72″ wide X 72″ high X 96″ deep  1500°F / 816ºC
 HT-205  48″ wide X 48″ high X 72″ deep  1400°F / 760ºC

Cryogenic Freezer Sizes

  Freezer#    Hot Zone Dimensions   Max Temperature   Max Load (lbs)
 DF-210
 60″ wide X 36″ high X 36″ deep
 -320°F / -160°C
 2500

Aluminum Drop Bottom Furnace

  Furnace#    Hot Zone Dimensions   Max Temperature   Max Load (lbs)
 HT-194
 60″ wide X 60″ high X 60″ deep
 1100°F / 593°C
 HT-195
 72″ wide X 72″ high X 72″ deep
 500°F / 260°C
 HT-196
 72″ wide X 72″ high X 72″ deep
 500°F / 260°C

Endothermic Furnaces

  Furnace#    Hot Zone Dimensions   Max Temperature   Max Load (lbs)
 HT-206
 24″ wide X 24″ high X 33″ deep
 1950°F / 1066°C
 HT-207
 24″ wide X 24″ high X 33″ deep
 1950°F / 1066°C

Vacuum Furnace Sizes

 Furnace #   Hot Zone Dimensions  Max Temperature  Max Load (lbs)
 HT-222  18″ wide X 18″ high X 36″ deep  2400°F / 1315°C  1,000
 HT-223  18″ wide X 18″ high X 36″ deep (all metal hot zone)  2400°F / 1315°C  1,000

Air Tempering Furnace Sizes

  Furnace #    Hot Zone Dimensions   Max Temperature   Max Load (lbs)
 HT-221  60″ wide X 48″ high X 168″ deep  1200°F / 649ºC  10,000

Freezer & Air Temper Furnace Size

  Furnace #    Hot Zone Dimensions   Min / Max Temperature   Max Load (lbs)
 HT-219
 43″ wide X 39″ high X 54″ deep
 -300°F / 1200°F  3,000