Solar Manufacturing Builds First Vacuum Oil Quench Furnace for Solar Atmospheres of Western PA
Hermitage PA, June 8, 2020 – Solar Atmospheres of Western PA (SAWPA) understands the need to expand their material hardening repertoire by adding oil quenching capabilities. The question has been – how to make this process safer and greener? The explosiveness of the protective endothermic gas along with the flammability of open oil quench tanks has provided concerns with regards to environmental, health and safety standards established by the SHARP recognition program. In 2019, Solar Manufacturing and Solar Atmospheres commenced engineering meetings with the goal to design and build a US manufactured, safe and quality vacuum oil quench furnace.
We are proud to announce a new Solar 36” x 36” x 48” Vacuum Oil Quench (VOQ) furnace, capable of safely quenching 2,000-pound loads without carbon potential concerns, will be operational in early 2021 at SAWPA.
SAWPA is currently constructing a 15,000 square foot building to make room for this VOQ furnace line. Besides the Solar VOQ furnace the additional equipment includes a parts washer, two tempering furnaces, and a charge car. The interconnecting 30’ tall building will be completed in mid-summer 2020, making the entire SAWPA complex 120,000 square feet under one roof.
For additional information about Solar Atmospheres of Western PA, contact Bob Hill at 1-855-934-3284 x2224, email at bob@solaratm.com, or visit us at www.solaratm.com.