New Titanium Drop Bottom Furnace Installation Underway
Hermitage PA, July 14, 2025 – The foundation is now in place at Solar Atmospheres of Western PA for the installation of a state-of-the-art titanium drop bottom water quench furnace. Engineered for precision and performance, this new furnace is rated for a maximum operating temperature of 1850°F ±10°F and is designed to process titanium bar and forging loads of up to 7,500 pounds.
Measuring 14 feet long by 54 inches wide by 48 inches high, workloads will be rapidly transferred into a 7,000-gallon, recirculated water quench tank within seconds—ensuring consistent metallurgical results for demanding aerospace and industrial applications.
This investment marks a significant step forward, opening the door to expanded titanium solution treating capabilities and reinforcing Solar Atmospheres’ commitment to innovation and customer-driven thermal processing solutions.
For additional information about Solar Atmospheres, contact Mike Johnson at 855-934-3284 x2223 or email at mikej@solaratm.com.