Solar Atmospheres of CA Increases Small Furnace Processing
To accommodate growing customer demand, Solar Atmospheres of California recently added some new equipment. The two new furnaces and freezer will assist in processing small to medium lots of parts made from metals ranging from PH grade stainless to Titanium.
- 2 Bar Vacuum Furnace – working zone of 12”W x 12”H x 22”L, operating temperatures range from 900°F to 2200°F. Capable of 2 bar quenching with nitrogen, argon, and helium.
- Air Temper Furnace – working zone of 21”W x 23”H x 23”L, operating temperatures range from 900°F to 1200°F
- Cryogenic Treatment Freezer – working zone of 12”W x 9”H x 27”L, operating temperatures range from -100°F to -300°F
President Derek Dennis explains, “More than ever, our customers are committed to streamlining their manufacturing processes through aggressive lean principle based programs. Since lead-time and delivery commitments are a very important part of eliminating waste, Solar plays a critical role in helping our customers achieve their goals. As a partner, rather than simply just another vendor in the approved supplier list, we have invested in this new processing equipment to speed turn-around, meet our customer’s evolving needs and contribute toward their success.”