Audio / Video

April 2016: Active Brazing of Titanium in a Vacuum Furnace

The April 2016 podcast is the third in the series about Vacuum Furnace Brazing. Our discussion centers on an overview of reactive brazing in a vacuum furnace and the use of active brazing alloys for successful results in joining titanium and titanium alloys.

Read More

February 2016: Vacuum Furnace Brazing of Stainless Steels

The February 2016 podcast is the second in the series about Vacuum Furnace Brazing. Our discussion centers on the advantages and concerns of brazing of Stainless Steel components with nickel-based and copper-based brazing alloys.

Read More

Vacuum Heat Treat Minute December 2015: The Advantages of Vacuum Furnace Brazing

This podcast is the first in a series on vacuum furnace brazing. It is an overview of the different types of brazing processes and why vacuum furnace brazing is superior to other joining methods, particularly torch brazing and welding.

Read More

Solar Atmospheres Vacuum Heat Treating Services

Tim Steber, Regional Sales Manager, gives an overview of vacuum heat treating processes at Solar Atmospheres during an interview at a Design 2 Part show in Oaks, PA.

Read More

Bob Hill Presents Webinar on How Additive Manufacturing May Change the Heat Treating World

Additive manufacturing (AM), commonly known as 3D printing, is the latest manufacturing technology taking the world by storm. Some people say AM will never replace traditional machining. Others believe it will change the world.

Read More

Vacuum Heat Treat Minute October 2015: Preventing Distortion and Cracking in a Vacuum Furnace

Distortion and cracking of parts is a common problem for heat treaters. This podcast is a discussion on how to prevent and reduce the distortion and cracking of tool steels and other ferrous alloys when cooling parts in a gas-quenching vacuum furnace.

Read More

Vacuum Heat Treat Minute August 2015: The Problem of Contaminated Ceramic Electrical Insulators in a Vacuum Furnace

This podcast features a discussion on how contaminants develop on ceramic insulators, how contamination affects the operation and performance of a vacuum furnace, and how to keep ceramic insulators clean of contaminants.

Read More

Vacuum Heat Treat Minute June 2015: Measuring and Monitoring Trace Levels of Dew Point and Oxygen in Quench Gases – Part 2

A discussion on the importance of measuring and monitoring the trace levels of dew point (water vapor), oxygen and other gases to reduce part contamination through the use of a residual gas analyzer for in-process vacuum analysis, research and development, and maintenance.

Read More

Vacuum Heat Treat Minute April 2015: Measuring and Monitoring Trace Levels of Dew Point and Oxygen in Quench Gases – Part 1

This month’s podcast is Part 1 on the importance of measuring and monitoring the trace levels of dew point and oxygen in quench gases to reduce part contamination while processing in a vacuum furnace.

Read More

Video: William Jones Presents Webinar on Vacuum Furnace Temperature Measurement

Heat transfer in a vacuum furnace takes place via radiation from the furnace heating elements to the workload being processed. Accurate temperature measurement of both the furnace hot-zone and the materials being processed is critical for a successful heat treat cycle.

Read More