Solar Atmospheres provides vacuum thermal processing for titanium material, parts, and weldments. With the world’s largest vacuum furnaces, 12, 24, 36 and 48 feet long, Solar is capable of vacuum processing furnace loads of bar, billet, sheet, and plate up to 150,000 pounds under 1X10-6 Torr vacuum levels. Specific heat treat services provided are: degassing, beta annealing, homogenizing, age hardening, creep forming, hydriding/dehydriding, stress relieving and Fluorescent Penetrant Inspection. Solar is Nadcap, ISO9001:2008 and AS9100C Registered and Boeing approved in heat treating, NDT (Non-destructive testing) services and BASCA (Beta Anneal Slow Cool Age). Solar Atmospheres serves customers with plants located in Pennsylvania, South Carolina, and California.