Author: Don Jordan, Solar Atmospheres
Claims for the benefits of cryogenic treatment abound. Research also abounds, but with differing conclusions. Yet, results have proven helpful, even dramatic, for the wear life of metal parts, dies and tooling applications after cryogenic treatment.